Combining XPS, ISS and REELS in one instrument provides the ideal system for quality control and experimentation of atomic layer depositions (ALD). In a recently published application note we investigate a series of samples consisting of thin layers of HfO2 deposited by increasing numbers of atomic layer deposition (ALD) cycles.
This experiment shows how Thermo Scientific™ Nexsa XPS System is able to quantify an amount of deposited hafnium, measure its thickness, its surface coverage and measure the band gap of the semiconductor material by combining three surface analysis techniques. This application note demonstrates how:
The Nexsa XPS System provides a complete picture of properties vital to the development of ultra-thin film materials for semiconductor applications.