Gold • Transition Metal

Primary XPS region: Au4f
Overlapping regions: N/A
Binding energies of common chemical states:

Chemical stateBinding energy Au4f7/2
Au metal84.0 eV

 

Experimental information
N/A
 
 
Interpretation of XPS spectra
  • Au4f region has well-separated spin-orbit components (Δ=3.7eV).
    • Peaks in the Au4f region have an asymmetric peak shape.
  • The Au4f7/2 peak can be a useful binding energy reference (Au4f7/2 at 84.00eV).
    • Binding energy shifts may be observed with Au nanoparticles, however.
      • Casaletto et al. analyzed Au nanoparticles on different metal oxide supports with XPS[1] and found two states of gold, Au0 and Au1+.
      • The Au1+ state was shifted by 2eV from the Au0 state.

 

Reference

[1] Casaletto et al., Surf. Interface Anal. 2006; 38: 215–218.

 

About this element
Element Crystal fcc

Symbol: Au
Date of discovery: circa 3000 BC
Name origin: Old English geolo
Appearance: gold
Discoverer: unknown
Obtained from: earth crust, copper ores

Melting point: 1337.58 K
Boiling point: 3080 K
Density[kg/m3]: 19300
Molar volume: 10.21 × 10-6 m3/mol
Protons/Electrons: 79
Neutrons: 118
Shell structure: 2,8,18,32,18,1
Electron configuration: [Xe]4f145d106s1
Oxidation state: 3,1
Crystal structure: cubic face centered

Gold, Latin aurium for "shining dawn", has been one of the most valued precious metals since prehistoric times and is mentioned several times in the Old Testament. Gold has been the standard for monetary exchange in many countries. While the metallic element takes on a yellow color en masse, when finely-divided it can also appear to be black, ruby, or purple in color. Being that gold is a soft metal, it is strengthened by being alloyed with other metals such as silver and copper. Gold’s heat and electrical conductivity qualities – as well as its resistance to heat, oxygen, moisture, and most corrosive agents – make it most applicable in coinage and jewelry. Seventy-five percent of all gold ever produced has been extracted since 1910. All gold ever refined would form a single cube twenty meters per side.

element_gold

Products

Nexsa G2 XPS

  • 微焦点 X 射线源
  • 独特的多技术选项
  • 用于单原子和簇离子深度剖析的双模式离子源
仪器卡片原件样式表

K-Alpha XPS

  • 高分辨率 XPS
  • 快速、高效、自动化的工作流程
  • 用于深度剖析的离子源

ESCALAB QXi XPS

  • 高光谱分辨率
  • 多技术表面分析
  • 丰富的样品制备和扩展选项

Contact us

Style Sheet for Global Design System
Style Sheet for Komodo Tabs
Style Sheet to change H3 to p with em-h3-header class
Style Sheet to change H2 style to p with em-h2-header class
产品表格规范样式表
Style Sheet for Global Design System
Style Sheet for Komodo Tabs
Style Sheet to change H3 to p with em-h3-header class
Style Sheet to change H2 style to p with em-h2-header class
产品表格规范样式表
Fix for left nav
支持和服务页脚样式表
字体样式表
卡片样式表

用于材料科学的
电子显微镜服务

为实现理想的系统性能,我们为您提供了由现场服务专家、技术支持部门和认证备件组成的全球网络支持。